Ideal for welding fine grained, cementation, tempered and cast steels where a minimum strength value of 830 N/mm2 is required.
Features and Applications
Suitability for use in welding fine-grained steels, cementation steels, tempered steels,
cast steels etc.
Suitability for use of applications requiring a minimum tensile strength value of 830 N/mm2
Requirement of re-drying for minimum 2 hours at the temperatures between of
300°C and 350°C
Typical Base Material Grades
HY 100, S690QL, S690QU, N-AXTRA 70
API 5L: X60, X65, X70, X80
Standards |
Current Type |
EN ISO 18275-A - E 69 5 Z Mn2NiCrMo B 4 2 H5
|
D.C.(+)
|
AWS A5.5 - E12018-G H4
|
|
Chemical Composition of Weld Metal % (Typical) |
C |
Si |
Cr |
Mo |
Ni |
Mn |
|
|
|
0.06 |
0.4 |
0.9 |
0.5 |
2.5 |
1.6 |
|
|
|
Mechanical Properties |
Yield Strength (N/mm2) |
Tensile Strength (N/mm2) |
Impact Strength (ISO-V/-50ºC)
|
Elongation (Lo=5do)(%) |
Heat Treatment |
min. 740
|
min 830-950
|
min. 28 J |
min. 17
|
560-600°C/1hr 300°C (air) |
Welding Positions

Operating Data |
Diameter x Length (mm) |
Welding Current (A) |
Package Weight (Kg) |
Carton Weight (Kg) |
3.50 x 350
4.00 x 450
5.00 x 450
|
90 - 140
130 - 190
170 - 240
|
5
6
6
|
15
18
18
|