Search
Filters
Close

GeKa - 8018-B3 OPUS 2 CML Electrodes (3.2mm) 2kg

Each
Availability: In stock
Order Code: 3010102410

Basic type electrode used for the welding of heat resisting steels containing 2¼ Cr - 1 Mo at elevated temperatures up to 600°C. Applications include piping, casting and boiler super heaters.

 

Features and Applications

Applicability in welding of heat-resisting steels containing 2% Cr - 1% Mn and similar alloys

Electrode with basic-type coating

Formation of more ductile and less hard weld metal due to low carbon content

Serviceability at temperatures of values up to 600 °C

Recommended pre-heating and post-heat treatment during welding processes

Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C

Vacuumed packed electrodes

 

Typical Base Material Grades

2% Cr - 1% Mo Steels, A335 Gr. P22

 

Standards Current Type
EN ISO 3580-A - E CrMo2L B 42 H5
D.C. (+)
AWS A5.5 - E8018-B3 L H4
 

 

Chemical Composition of Weld Metal % (Typical)
C Si Mn  Mo Cr
0.04 0.6 0.6 1.1
2.2

 

Mechanical Properties
Yield Strength
(N/mm2)
Tensile Strength
(N/mm2)

Impact Strength
(ISO-V/-50ºC)

Elongation
(Lo=5do)(%)
Heat Treatment
min. 530
min 620
min. 47 J min. 18
690-750ºC/1hr
300ºC (air)

 

Welding Positions

 

 

Operating Data
Diameter x Length (mm) Welding Current (A) Package
Weight (Kg)
Carton
Weight (Kg)

2.50 x 350

3.20 x 350

4.00 x 450

80 - 110

100 - 140

130 - 180

2

2

3

12

12

18

Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained. This information is subject to change without notice and can be only considered as suitable for general guidance.

Basic type electrode used for the welding of heat resisting steels containing 2¼ Cr - 1 Mo at elevated temperatures up to 600°C. Applications include piping, casting and boiler super heaters.

 

Features and Applications

Applicability in welding of heat-resisting steels containing 2% Cr - 1% Mn and similar alloys

Electrode with basic-type coating

Formation of more ductile and less hard weld metal due to low carbon content

Serviceability at temperatures of values up to 600 °C

Recommended pre-heating and post-heat treatment during welding processes

Requirement of re-drying for min. 2 hours at the temperatures between 300°C and 350°C

Vacuumed packed electrodes

 

Typical Base Material Grades

2% Cr - 1% Mo Steels, A335 Gr. P22

 

Standards Current Type
EN ISO 3580-A - E CrMo2L B 42 H5
D.C. (+)
AWS A5.5 - E8018-B3 L H4
 

 

Chemical Composition of Weld Metal % (Typical)
C Si Mn  Mo Cr
0.04 0.6 0.6 1.1
2.2

 

Mechanical Properties
Yield Strength
(N/mm2)
Tensile Strength
(N/mm2)

Impact Strength
(ISO-V/-50ºC)

Elongation
(Lo=5do)(%)
Heat Treatment
min. 530
min 620
min. 47 J min. 18
690-750ºC/1hr
300ºC (air)

 

Welding Positions

 

 

Operating Data
Diameter x Length (mm) Welding Current (A) Package
Weight (Kg)
Carton
Weight (Kg)

2.50 x 350

3.20 x 350

4.00 x 450

80 - 110

100 - 140

130 - 180

2

2

3

12

12

18

Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained. This information is subject to change without notice and can be only considered as suitable for general guidance.