Features and Applications
A copper coated heat-resisting wire containing 0.5% molybdenum.
Designed for welding low alloy creep resistant steels that require a high tensile strength.
Weld deposit highly resistant to cold cracking.
Recommended working temperatures of up to 500°C.
Typically used on creep steels for construction steam boilers, pressure tanks, gas pipes, shipbuilding sector, petrochemical industry, heat exchangers, building of cranes, bridges etc.
Green wire is produced using virgin raw materials sourced from specialised steel mills, which ensures consistent reliability and quality.
Test Certificates can be found online @wilkinsonstar247.com
Typical Base Materials
P295GH, P355GH, 16Mo3, 17Mo3, 14Mo6, S275, S355, S420, A210, A285, A335, A516, S275Ml, S355M, S420M, S460 15Mo3, 10MnMo45, 11MnMo45, GS60, GS22Mo4, 20MnMoNi5-5, 15NiCuMoNd5S, 17MnMoV64*
* Illustrative, not exhaustive list
Standards |
EN ISO 636-A - W 2Mo
|
AWS A5.28 - ER 70S-A1
|
Chemical Composition % (Typical) |
C% |
Si% |
Mn% |
P% |
S% |
Cu% |
|
0.09 |
0.60 |
1.20 |
<0.015 |
<0.015 |
<0.25 |
|
|
|
|
|
|
|
|
Cr% |
Ni% |
Mo% |
Al% |
V% |
Zr+Ti% |
|
<0.15 |
<0.10 |
0.50 |
<0.030 |
<0.020 |
<0.050 |
|
Mechanical Properties (Typical)
|
Tensile Strength |
610 MPa |
|
Yield Strength |
520 MPa
|
|
Elongation |
25% |
|
Impact Strength |
150 J |
>47 J
|
Test Temperature |
+20ºC |
-40ºC |
Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.
Shielding Gases
EN ISO 14175 - TIG: I1 (Argon)
Welding Positions
EN ISO 6947 - PA, PB, PC, PD, PE, PF
Packaging Data |
Diameter
|
Length
|
Weight |
|
1.60 mm
2.40 mm
3.20 mm
|
1000 mm
1000 mm
1000 mm
|
5 Kg
5 Kg
5 Kg
|
|
Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained, this information is subject to change without notice and can be only considered as suitable for general guidance.