Features and Applications
Solid wire suitable for welding weather resistant structural steels like Corten and other high strength low-alloy steels.
Alloyed with copper and nickel which gives a high resistance against atmospheric corrosion.
This wire provides a unique aesthetic appeal and can be identified by its typically reddish rust or patina look for structural and artistic applications.
Typically used on the construction of containers, tanks, bridges, building panels, chimneys, means of transport, offshore platforms etc.
Green wire is produced using virgin raw materials sourced from specialised steel mills, which ensures consistent reliability and quality.
Test Certificates can be found online @wilkinsonstar247.com
Typical Base Materials
S235JRW, S235J2G3 ; Patinax 37, Alcodur50, Koralpin 52, ; S355J2G3Cu, 9CrNiCuP3-2-4 ; Corten A - B1 ; TsT52.3, S355K2W*
* Illustrative, not exhaustive list
Standards |
EN ISO 636-A - W Z3Ni1
|
AWS A5.28 - ER 80S-G
|
Chemical Composition % (Typical) |
C% |
Si% |
Mn% |
P% |
S% |
Cu% |
0.08 |
0.80 |
1.40 |
<0.020 |
<0.020 |
<0.40 |
|
|
|
|
|
|
Cr% |
Ni% |
Mo% |
Al% |
V% |
Zr+Ti% |
0.25 |
0.80 |
<0.05 |
<0.200 |
<0.030 |
<0.15 |
Mechanical Properties (Typical)
|
Tensile Strength |
630 MPa |
|
Yield Strength |
550 MPa
|
|
Elongation |
22% |
|
Impact Strength |
60 J |
|
Test Temperature |
-40ºC |
|
Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.
Shielding Gases
EN ISO 14175 - TIG: I1 (Argon)
Welding Positions
EN ISO 6947 - PA, PB, PC, PD, PE, PF
Packaging Data |
Diameter
|
Length
|
Weight |
1.60 mm
2.40 mm
3.20 mm
|
1000 mm
1000 mm
1000 mm
|
5 Kg
5 Kg
5 Kg
|
Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained, this information is subject to change without notice and can be only considered as suitable for general guidance.